      GENIA 83  
 
GENIA117
Master alloy suitable for the production of 585‰ pink gold alloys (Cu75Zn5). This gold alloy lends itself for the production of stamped items, solid and hollow chains, earrings, bracelets and tube rings. This gold alloy lends itself for hardening. It can be used with all casting methods (mould casting and continuous casting).
GENIA117 - (585) ***************
GENIA117 - (585) ******************************************
+
+
+
GENIA119
Master alloy suitable for the production of 375‰ and 417‰ yellow gold alloys (Ag10Zn19). This gold alloy lends itself for the production of stamped items, solid and hollow chains, earrings, bracelets and tube rings. It is not suitable for hardening, therefore its use is recommended only when high hardness (>150HV) is not required in the final product. It can be used with all casting methods (mould casting and continuous casting).
GENIA119 - (875) ****************
GENIA119 - (375) *************************************
GENIA119 - (417) *************************************
GENIA119 - (875) ***************************************
+
+
+
GENIA120
Master alloy suitable for the production of 585‰ yellow gold alloys (Ag5Zn23). The resulting alloy is for the production of stamped items, solid and hollow chain, earrings, bracelets and tube rings. Its use is recommended only when high hardness (>150HV) is not required in the final product; this alloy is not suitable for hardening. It can be used with all casting methods (mould casting and continuous casting).
GENIA120 - (585) ************************************
+
+
+
GENIA121
Master alloy suitable for the production of 375‰ and 417‰ yellow gold alloys. This gold alloy lends itself for the production of stamped items, solid and hollow chains, earrings, bracelets and tube rings. The gold alloy is not suitable for hardening, therefore its use is recommended only when high hardness is not required in the final product. This alloy is not suitable for hardening. It can be used with all casting methods (mould casting and continuous casting).
GENIA121 - (375) ************************************
GENIA121 - (417) ************************************
+
+
+